China Mold

Cooling Water Conditions For Plastic Mold Processing

Cooling Water Conditions For Plastic Mold Processing

Conditions for cooling water for plastic mold processing
1. The water transport margin and product material margin are generally not less than 10MM, and should be designed between 10MM-12MM as much as possible; the alloy mold is generally 25MM;
2, the water delivery margin and the margin settings of the insert needle, thimble, cylinder, insert material are as follows:

3. The water transport, gas cap and oil pressure circuit are not less than 8MM;
4. the water transport side and the mouth side of the mouth are not less than 8MM:
5. the water transport side and the inner mold side are not less than 10MM;
6. the distance design of water transportation and water transportation in the same direction:

7.the edge of the rubber ring of the water barrier is not less than 2MM; the throat plug and the throat plug are not less than 5MM;
8. Generally, no more than 8 spacers are connected in series for each water transportation circuit, (American fisherman customers require no more than 6 spacers in series;)
9, when designing the cooling water of the insert, the closest distance between the transport water and the material level of the insert should be 5MM;